Coated item |
Color |
Application |
Performance parameter |
AD12 |
Black
 |
For viscous materials, aluminum, acrylic, polyethylene, carbon fiber materials |
Nano Hardness: HV2200, Friction Coefficient: 0.2 Max.Temp: 400° |
AT12 |
Gold
 |
Universally used for materials within HRC45, iInclude the following materials: stainless steel, 303, 316F, Nickel stainless steel, etc.; steel hardened steel, molybdenum steel, fierce steel and other carbon steel; Pig iron, cast iron, nickel alloy, acrylic |
Nano Hardness: HV3500, Friction Coefficient: 0.3 Max.Temp: 900° |
AL25 |
Bule grey
 |
Low carbon materials, pure iron, low carbon steel and low carbon stainless steel, such as 304 stainless steel |
Nano Hardness: HV3500, Friction Coefficient: 0.25 Max.Temp: 800° |
AT25 |
Black
 |
Carbon steel, alloy steel, bearing steel, hardened steel, Cr-Mo stee, manganese steel |
Nano Hardness: HV3500, Friction Coefficient: 0.6 Max.Temp: 900° |
JS25 |
Bronze
 |
Widely used in materials within HRC60, include the following materials: austenitic/martensitic stainless steel, 316L, 303, 321, 316F, high nickel stainless steel, etc.; steel (bearing steel, hardened steel, pig iron, Chromium-molybdenum alloy steel, high carbon steel such as manganese steel) cast iron, nickel alloy, etc. |
Nano Hardness: HV4500, Friction Coefficient: 0.4 Max.Temp: 1100° |
TZ25 |
Champagne gold
 |
Special use for titanium alloy. |
Nano Hardness: HV4000, Friction Coefficient: 0.55 Max.Temp: 900° |